A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Dissolving Gold electrodes
Dissolving Gold electrodes
2002-08-21
Jeroen Nieuwenhuis
2002-08-21
David Nemeth
2002-08-22
Heiko van der Linden
2002-08-22
Dr. Stefan Fiedler
2002-08-22
Christopher Blanford
2002-08-21
Tabada, Phillipe
2002-08-22
Nico Visch
Dissolving Gold electrodes
Heiko van der Linden
2002-08-22
Hi Jeroen,

I have had this problem too, but at higher voltages.
If the voltage becomes too high chlorine gas will be
generated from the chloride ions that attacks the gold.
I would check the voltages with an oscilloscope.
And of course if you have a material under your gold
maybe this is lifted off of your substrate causing
the gold to be "dissolved"

I hope this helps,
Heiko

*******************************
MESA+ Research Institute
      Twente University
         P.O. Box 217
     7500 AE Enschede
       The Netherlands
*******************************


-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Jeroen Nieuwenhuis
Sent: Wednesday, August 21, 2002 6:30 PM
To: [email protected]
Subject: [mems-talk] Dissolving Gold electrodes


Dear all,

I am trying to measure the impedance of a 1% NaCl solution using 50 um x
150 um gold electrodes (thickness 0.6 um) in a microchannel and the
electrodes dissolve in about 40 minutes(!).

I used very pure NaCl and distilled water to make the solution. I use a
sine-wave generator to make a 50 mV AC voltage (offset oV) and I measure
the current using an transimpedance-amplifier with a 100k resistor. Nor
the source nor the read-out electronics seems to generate a DC value
current.

Does anybody have a suggestion what is going on? To the best of my
knowledge nothing should happen when the AC voltage used is less than
about a volt.

Regards,
Jeroen Nieuwenhuis _______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
MEMS Technology Review
Nano-Master, Inc.