MEMSnet Home: MEMS-Talk: Ti O2 on SiNx
Ti O2 on SiNx
2002-08-21
Haigh, Richard
2002-08-21
Roger Shile
2002-08-22
[email protected]
Ti O2 on SiNx
Roger Shile
2002-08-21
Was the SiNx deposited by PECVD?
If so it likely contained a lot of hydrogen which would outgas during the
oxidation and create bubbles under the metal.  A solution might be to outgas
the hydrogen at 600 C or higher prior to depositing the metal.

Roger Shile

-----Original Message-----
From: Haigh, Richard [mailto:[email protected]]
Sent: Wednesday, August 21, 2002 9:06 AM
To: [email protected]
Subject: [mems-talk] Ti O2 on SiNx


I have deposited Ti (80 nm) onto SiNx (200 nm) on Si. The Ti was then
oxidised at 600 C. Bubbles have formed on the surface of the TiO2
following oxidation. Has anyone experienced a similar effect?

Regards


Richard Haigh
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
"This email and any attachments may contain information that is confidential and
proprietary information of Veeco Instruments Inc. and are intended only for the
use of the addressee. Unauthorized use, distribution or copying is forbidden. If
you have received this email in error, please notify the sender immediately by
return email and delete all copies of this message and any attachments from your
computer. Thank you."

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering