A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SOI wafer needed and one question about soi
SOI wafer needed and one question about soi
2002-08-21
weibin zhang
2002-08-22
Andrew Kuchling
2002-08-22
Lawlor, Chris
2002-08-22
Blunier, Stefan
SOI wafer needed and one question about soi
Blunier, Stefan
2002-08-22
You can ask

Sico Meiningen Wafer GmbH
Jerusalemerstr. 13
D-98611 Meiningen
Germany
Tel 011 49 3693 71313
Fax 011 49 3693 71315
e-mail: [email protected]

Greetings
Stefan

-----Original Message-----
From: weibin zhang [mailto:[email protected]]
Sent: Mittwoch, 21. August 2002 20:27
To: [email protected]
Subject: [mems-talk] SOI wafer needed and one question about soi


Hi,all

I need some SOI wafer for my processing.  Can someone give any information?
I
need the device layer should be well conductive. Does anyone has any idea
what
is the maximum resistivity should that require?

other specifications for the soi wafer :

device layer:   15-50 microns
box layer :     > 1 micron
substrate :  resistivity >> resistivity of device layer

thanks

weibin
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

[demime 0.98e removed an attachment of type text/x-vcard which had a name of
Blunier, Stefan.vcf]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Harrick Plasma, Inc.
University Wafer