A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Tantalum nitride etch
Tantalum nitride etch
2002-08-21
Peter & Judy Wright
2002-08-27
Neal Ricks
2002-08-28
Oray Orkun Cellek
2002-08-28
Peter & Judy Wright
2002-08-21
Tabada, Phillipe
2002-08-29
Michael Yakimov
Tantalum nitride etch
Oray Orkun Cellek
2002-08-28
The reference , M. Kohler, "Etching in Microsystem Technology ", Wiley,1999
gives an etchant without HF:

NaOH 7 mol/l
H2O2 0.9 mol/l
Temp : 90 C
Rate : 1.7 .. 3.3 nm/s

Oray Orkun Cellek
[email protected]
Middle East Technical Univ.
EE Dept.
Ankara
Turkey

----- Original Message -----
From: "Neal Ricks" 
To: 
Sent: Tuesday, August 27, 2002 11:19 PM
Subject: Re: [mems-talk] Tantalum nitride etch


> Have you tried the published Tantalum etches, or do you have to avoid use
of HF?
>
>
>  Peter & Judy Wright
> wrote:Does anyone know of a wet etch for tantalum nitride? We are using it
for an
> underbump metalization at a subcontractor who does not have a dry etch
> capability.
>
> Peter Wright
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
> Yahoo! Finance - Get real-time stock quotes
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
The Branford Group