Hello,
   Im looking at etchants for microstructural analysis
of 63/37 Sn/Pb solder joints. i had used Hydrogen
peroxide and Ammonium hydroxide for the etchign but
still the SEM image does not clearly distinguish the
Tin and lead matrix. Can anybody suggest ways to
clearly distinguish the metallurgy and the
intermetallics?

thanks,
VIJAY,
RIT, NY.


__________________________________________________
Do You Yahoo!?
Yahoo! Finance - Get real-time stock quotes
http://finance.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation