MEMSnet Home: MEMS-Talk: Nickel etchant
Nickel etchant
2002-09-09
Phaneendra Medida(fabbi)
2002-09-09
David Nemeth
2002-09-09
Neal Ricks
2002-09-10
David Nemeth
2002-09-09
Neal Ricks
2002-09-09
Kishan Gupta
2002-09-10
Neal Ricks
2002-09-10
Kishan Gupta
Nickel etchant
David Nemeth
2002-09-09
In my experience, this solution will not attack Nickel that is not in
contact with another metal.  It will aggressively attack nickel that is
sandwiched between two layers of gold (don't ask me why - go ask an
electrochemist).  It will sometimes attack nickel that is on top of gold,
depending on the deposition method of the Nickel.

David Nemeth
Senior Process Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Phaneendra Medida(fabbi)
Sent: Monday, September 09, 2002 2:47 PM
To: [email protected]
Subject: [mems-talk] Nickel etchant


Does this solution (KI(Potassium iodide)+I2(Iodine)+Water) Etch Nickel?

Fabbi.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing
University Wafer