you would do best to talk directly with Craig Shuckert of HDMicrosystems,
Wilmington DE

if you cant find it, let me know and I will send his contact info

Robb

!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!
!!!!!!!!!!!!!!!!
Please note the change in email address shown below.
Use the email address below for all correspondence.
! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! ! !
! ! ! ! ! ! ! ! ! ! ! ! ! ! !


Robb White
Chief Scientist, Technology Development Laboratories
Science Applications International Corporation (SAIC)
1710 SAIC Dr., MS 2-3-1
McLean, VA 22102

Phone: 703-676-6384
Fax: 703-676-5509
email: [email protected]


-----Original Message-----
From: Zhimin J Yao [mailto:[email protected]]
Sent: Monday, September 09, 2002 3:48 PM
To: [email protected]
Subject: [mems-talk] Polyimide for plannarization


Hello,

I need a polyimide that has a better than 50% degree of plannarization,
about 3 microns thick.  Wet etchable preferred.  Can anyone tell me where I
can find it?  I have checked HDmicrosystem's web page.

Thanks,
Z. Jamie Yao


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group
Nano-Master, Inc.