MEMSnet Home: MEMS-Talk: residue after etching doped oxide
residue after etching doped oxide
2002-09-17
Yahong Yao
2002-09-18
Robert C Cole
2002-09-18
[email protected]
residue after etching doped oxide
Yahong Yao
2002-09-17
Hey Colleagues,

Recently, I observed residue after etching doped oxide by HF.  Two kinds of
films:

1. PSG deposited by LPCVD.  This film is used as the sacrificial layer.
After etching by HF (49%), a blanket-sheet-like residue stays on the sample
surface.  This can be removed by Piranha but Piranha is not good for my
device at this point.

2. Phosphorous doped LTO.  This film also leaves residue on the sample
surface after etched by HF.  This residue is not like a blanket.  There are
some spots sticking on pattern edges.

Did anybody come across the same problem?  Any help is highly appreciated.
Thanks.

Yahong

_________________________________________________________________
Chat with friends online, try MSN Messenger: http://messenger.msn.com



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review