MEMSnet Home: MEMS-Talk: looking for single wafer LPCVD nitride services
looking for single wafer LPCVD nitride services
2002-09-17
Robert J. Kogut
2002-09-17
bille@npphotonics (Bill Eaton)
2002-09-19
Rohit Srivastava
2002-09-18
Schuurman, Gilbert
looking for single wafer LPCVD nitride services
Schuurman, Gilbert
2002-09-18
Lionix (http://lionphotonix.nl) might be able to help you.

Gilbert

-----Original Message-----
From: Robert J. Kogut [mailto:[email protected]]
Sent: dinsdag, 17 september 2002 21:09
To: [email protected]
Subject: [mems-talk] looking for single wafer LPCVD nitride services


I'm looking for a vendor who will do LPCVD nitride deposition on single
wafers or small quantities.  I only have a few 4 inch wafers to be
coated; I'd rather not pay for a whole 25 wafer run.


 -Bob Kogut





_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.