Robert J. Kogut
2002-09-17
bille@npphotonics (Bill Eaton)
2002-09-19
Rohit Srivastava
2002-09-18
Schuurman, Gilbert
looking for single wafer LPCVD nitride services
Rohit Srivastava
2002-09-19
Hi,
   We recently got LPCVD polysilicon deposited from
Case Western at a very reasonable price. Try emailing
Alex Smith at
[email protected]
for a quote.
Thanks
Rohit
IfM
Louisiana Tech University
Ruston, LA 71272


--- "bille@npphotonics (Bill Eaton)"
 wrote:
> The trouble with single wafer service is that
> usually LPCVD is an inherently
> batch process. Hence the cost to the foundry is the
> same for 1 wafer as it
> is for 25.
>
> >
> > I'm looking for a vendor who will do LPCVD nitride
> deposition
> > on single
> > wafers or small quantities.  I only have a few 4
> inch wafers to be
> > coated; I'd rather not pay for a whole 25 wafer
> run.
> >
>
> Bill Eaton, Ph.D.
> Materials & Analysis Manager
> NP Photonics
> 5706 Corsa Avenue, Suite 100
> Westlake Village, CA  91362
> Voice:  (818) 991-7044 x211
> eFax:   (503) 214-5559
> mailto://[email protected]
> www.parvenutech.com
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/


__________________________________________________
Do you Yahoo!?
New DSL Internet Access from SBC & Yahoo!
http://sbc.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing