Dear Ton van Helvoort:

Thank you  for the information.

Wenlin jin





"Antonius Helvoort" @memsnet.org on 09/21/2002
05:17:00 AM

Please respond to [email protected]

Sent by:  [email protected]


To:   [email protected]
cc:
Subject:  Re: [mems-talk] anodic wafer bonding


Dear Wenlin Jin,

Hope these references, discussing damage due to E-field will be of used to
you (and others):

 SchjØlberg-Henriksen K., Plaza J.A., Rafí J.M., Esteve J., Campabadal F.,
Santander J., Jensen G.U. and Hanneborg A., "Protection of MOS capacitors
during anodic bonding", Journal of Micromechanics and Microengineering, 12,
361-367, 2002

 SchjØlberg-Henriksen K., Hanneborg A.B., Jensen G.U., Lapadatu A.C. and
Jakobsen H., "Electrical effects of anodic bonding on silicon dioxide
situated in Pyrex cavities", Journal of the Electrochemical Society, 149,
G497-G503, 2002.

 Li Z., Hao Y., Zhang D., Li T. and Wu G., " An SOI-MEMS technology using
substrate layer and bonded glass as wafer-level package", Sensors and
Actuators, 96, 34-42, 2002.

       Cozma, A., Jakobsen, H. and Puers, R.,"Electrical characterization
of anodically bonded wafers", Journal of Micromechanics and
Microengineering, 8, p 69-73, 1998.



Cambridge, UK

>From: [email protected]
>Reply-To: [email protected]
>To: [email protected]
>Subject: [mems-talk] anodic wafer bonding
>Date: Wed, 11 Sep 2002 08:45:15 -0400
>
>Hello:
>
>In anodic bonded chips, there exist electric charges in the bonding area.
>If the chip is an electro-static device, will these charges interact with
>electrical voltage applied?
>
>Your help is highly appreciated.
>
>Wenlin Jin
>
>
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/




_________________________________________________________________
Send and receive Hotmail on your mobile device: http://mobile.msn.com


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
University Wafer
Nano-Master, Inc.