Edges problem in through-mask NiFe electroplating
Mike Mattes
2002-10-17
Magali,

I would recommend injecting some negative pulses into your plating current. You
will have to do some experimenting to see what the amplitude and frequency
should be, however, that should work.

Regards,
Mike Mattes
Medtronic, Inc.

>>> [email protected] 10/17/02 12:58AM >>>
Dear all,

On a silicon wafer where a Cu seed layer is sputtered, I am depositing
photoresist (8um thick) to create patterns and then electroplating  NiFe
through the patterns (5um thick).

The deposit has an even thickness except at the edges where there is a
big overplating. (kind of
"dog hears")

Does anyone have an idea on how to get rid of this edge problem?

Thanks a lot in advance,

Magali
--
PEI Technologies,
NMRC, Lee Maltings, University College,
Cork, Ireland.

Tel: +353 21 4 904279
Fax: +353 21 4 270271
email: [email protected]



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
University Wafer