In addition to the LIGA capability you mentioned at MCNC/Wisconsin, a west
coast LIGA team has been formed with members from the Jet Propolsion Laboratory
(JPL), Lawrence Berkeley National Lab (LBNL), Sandia National Lab (SNL),
Lawrence Livermore National Lab (LLNL) and the Stanford Synchrotron Radiation
Lab (SSRL). This group is addressing a variety of projects including fine pitch
grids, motor components and micro instruments. For further information on the
acitivities of this group contact Dean Wiberg at:

[email protected] (510) 486 4900

Date: 8/7/95 10:28 PM
To: Dean Wiberg
From: [email protected]
Check with Prof. Friedrich (I think that's the name) at Louisiana State
University's Institute for Micromanufacturing (IfM); they use very small steel
and silicon based tools to mill (yes, mill) structures such as you wish.

Or, use the LIGA process through MCNC and the UWisconsin (Prof. Guckel).

Al


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing