Hi everyone,
I am using a three step etching process to obtain deep silicon structures.
During the process, I used H2 and CF4 to generate teflon layer to
passivate the sidewalls during the etching. After wet etching of the
sacrifical layer, I used critical dryer to dry my sample. However, strange
situation happened after the drying: all the deposited teflon layers come
off from the sidewalls, and make all the things really messy. Does anyone
of you know how to deal with this problem? I am wondering if there is any
solvent to dissolve the teflon layers.
Thanks for any help or suggestion!

Peng Yao
DOEs lab
Electrical Engineering Dept.
Univeristy of delaware
Newark D.E 19716



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
MEMStaff Inc.
Addison Engineering