A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Bonding material impervious to KOH bath
Bonding Si to Si
2002-10-31
Josef Kouba
2002-11-01
CLIF HAMEL
2002-11-01
Luesebrink Helge
2002-11-01
Jeff Birkmeyer
2002-11-01
Kenneth Smith
2002-11-04
Josef Kouba
Bonding material impervious to KOH bath
2002-11-02
[email protected]
2002-11-04
Atzmon Ofri
Bonding material impervious to KOH bath
[email protected]
2002-11-02
Are there materials that can used for wafer bonding
that doesn't get etched/stripped in KOH bath? I've
already tried Apiezon black wax, crystal bond, SU-8
(not fully crossed), but they all seems to not work
quite well. I would appreciate any advice.
Thanks,
Kevin


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
University Wafer
Tanner EDA by Mentor Graphics