Hi. I have a problem with a notching from wet etching. I am trying to
pattern and etch 20um LTO line and 20um aluminum line patterned over
polysilicon step. After etching, I see a side notching on both LTO and
aluminum line at the polysilicon step (metal deposited and etched then LTO
is patterned). I check the step coverage of LTO, aluminum, and photoresist
after hardbake and they all look fine under SEM. The notching seems to occur
underneath the resist under microscope.
Does anybody ever had similar problem?
Thank you
Ken

_________________________________________________________________
Add photos to your e-mail with MSN 8. Get 2 months FREE*.
http://join.msn.com/?page=features/featuredemail



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.
MEMS Technology Review