Hello everyone,
I am etching my mask using a wet chemical etch, my main concern is the under
etch during the mask making.
I am interested in the max. achievable CD. 0.8 - 1 micron slits (glass
lines)
I there any tricks and tip in general you can give me?
Does anybody know a Cr dry-etch service in Europe for 6" reticle. (fast)
Best regards,
Marc van den Boogaart



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Mentor Graphics Corporation
The Branford Group