MEMSnet Home: MEMS-Talk: How to remove PDMS sticiing to the Si mold etched by DRIE?
How to remove PDMS sticiing to the Si mold etched by DRIE?
2002-11-20
[email protected]
2002-11-20
Hyoung Jin "Joe" Cho
2002-11-20
Christopher Blanford
2002-11-21
Alison Cleary
2002-11-21
Likun Zhu
2002-11-21
Hyoung Jin "Joe" Cho
2002-11-20
Phillipe Tabada
How to remove PDMS sticiing to the Si mold etched by DRIE?
Hyoung Jin "Joe" Cho
2002-11-20
PDMS can be removed chemically with Dynasolve 210 or Dynasolve 218.
Contact:
Dynaloy, Inc.
PO Box 33609
1910 S. State Av.
Indianapolis, IN 46203
800-669-5709

Sincerely,

______________________________
Hyoung Jin "Joe" Cho, Ph.D.
Assistant Professor
Mechanical, Materials & Aerospace Engineering
University of Central Florida, Orlando, FL 32816-2450
(Office) 407-207-7245
(Fax) 707-202-2978
(Web) http://mmae.ucf.edu/~joecho
(Email)[email protected]
(Email)[email protected]
********NanoFab & BioMEMS********

<<<
(O-O)  o0O  Imagination is more important
(_3_)            than knowledge.
d-v-b              -Albert Einstein




-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of [email protected]
Sent: Wednesday, November 20, 2002 3:52 PM
To: [email protected]
Subject: [mems-talk] How to remove PDMS sticiing to the Si mold etched
by DRIE?


Deal MEMS reserachers:

        I got a problem when peel off PDMS off the Si mold made by DRIE
since I
did not treat the mold before pour PDMS on. After that, I tried to use HF to
remove PDMS so that I can use the mold again. But it takes very long and the
cleaning is not complete. Can anybody give some suggestions how to totally
remove the PDMS from the Si mold? Any input is highly appreciated.



Sincerely,

Bo




_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
MEMStaff Inc.
Mentor Graphics Corporation