Alison Cleary
2002-11-21
Likun Zhu
2002-11-21
Hyoung Jin "Joe" Cho
2002-11-20
Phillipe Tabada
How to remove PDMS sticiing to the Si mold etched by DRIE?
Phillipe Tabada
2002-11-20
Hi Bo,

   If you have access to an STS system, I would recommend a 30sec to 2 min
exposure of the passivation gases only which will coat your Si mold with a
teflon like material and make it alot easier for the PDMS to come off.
However, the teflon coat does breakdown after subsequent moldings and will
have to be removed using plasma or HF and recoated.

Phil






>From: [email protected]
>Reply-To: [email protected]
>To: [email protected]
>Subject: [mems-talk] How to remove PDMS sticiing to the Si mold etched by
>DRIE?
>Date: Wed, 20 Nov 2002 14:51:56 -0600 (CST)
>
>Deal MEMS reserachers:
>
>         I got a problem when peel off PDMS off the Si mold made by DRIE
>since I
>did not treat the mold before pour PDMS on. After that, I tried to use HF
>to
>remove PDMS so that I can use the mold again. But it takes very long and
>the
>cleaning is not complete. Can anybody give some suggestions how to totally
>remove the PDMS from the Si mold? Any input is highly appreciated.
>
>
>
>Sincerely,
>
>Bo
>
>
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/


_________________________________________________________________
MSN 8 helps eliminate e-mail viruses. Get 2 months FREE*.
http://join.msn.com/?page=features/virus



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.