A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: special photolithography needed
special photolithography needed
2002-11-20
Enzhu Liang
2002-11-20
X. Yuan
2002-11-20
Christopher Blanford
2002-11-20
Greg Miller
2002-11-20
Bill Moffat
2002-11-20
BERAUER,FRANK (HP-Singapore,ex7)
2002-11-21
Alex Pozdin
special photolithography needed
BERAUER,FRANK (HP-Singapore,ex7)
2002-11-20
Bill Moffat wrote:
>       This could be difficult.  A possible but expensive answer
> may be a 3D Holographic projection aligner.  Karl Suss used to
> manufacture one this gives you the ability to use a variable
> focus and expose with the same intensity at different focal
> lengths from the mask plane.  If you need more information I
> can probably locate engineers who have used this sort of system
> for exposure down the side of a steeply sloping line with the
> same C.D. at the top, down the slope, and at the bottom of the
> slope.  Bill Moffat

We have done multiple step exposure with different focus heights
(and multiple masks) to pattern lines on anisotropically etched
slopes (up to 350um depth, but the method can theoretically be
used on any depth) with very good CD results. We used a modified
UTS stepper and have a patent on this.
Please contact me for more details and publications if needed.

Greetings,
        Frank Berauer
        Senior R&D Engineer
        Hewlett-Packard Singapore


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics