How to remove PDMS sticiing to the Si mold etched by DRIE?
2002-11-20
[email protected]
2002-11-20
Hyoung Jin "Joe" Cho
2002-11-20
Christopher Blanford
2002-11-21
Alison Cleary
2002-11-21
Likun Zhu
2002-11-21
Hyoung Jin "Joe" Cho
2002-11-20
Phillipe Tabada
How to remove PDMS sticiing to the Si mold etched by DRIE?
Alison Cleary
2002-11-21
Dear Bo,

I believe that Toluene will dissolve PDMS if you leave it overnight,
although I haven't verified this myself. Maybe someone else out there
can confirm this...

Good luck!
Alison

[email protected] wrote:

>Deal MEMS reserachers:
>
>        I got a problem when peel off PDMS off the Si mold made by DRIE since I
>did not treat the mold before pour PDMS on. After that, I tried to use HF to
>remove PDMS so that I can use the mold again. But it takes very long and the
>cleaning is not complete. Can anybody give some suggestions how to totally
>remove the PDMS from the Si mold? Any input is highly appreciated.
>
>
>
>Sincerely,
>
>Bo
>
>
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
>

--
Alison Cleary
Bioelectronics Group
Electronics and Electrical Engineering
Oakfield Avenue
University of Glasgow
G12 8LT
Scotland
UK

Phone: +44 (0)141 330 2092





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing