MEMSnet Home: MEMS-Talk: How to remove PDMS sticiing to the Si mold etched by DRIE?
How to remove PDMS sticiing to the Si mold etched by DRIE?
2002-11-20
[email protected]
2002-11-20
Hyoung Jin "Joe" Cho
2002-11-20
Christopher Blanford
2002-11-21
Alison Cleary
2002-11-21
Likun Zhu
2002-11-21
Hyoung Jin "Joe" Cho
2002-11-20
Phillipe Tabada
How to remove PDMS sticiing to the Si mold etched by DRIE?
Likun Zhu
2002-11-21
Try nanostrip.
I used it to remove PDMS.

--- Alison Cleary  wrote:
> Dear Bo,
>
> I believe that Toluene will dissolve PDMS if you
> leave it overnight,
> although I haven't verified this myself. Maybe
> someone else out there
> can confirm this...
>
> Good luck!
> Alison
>
> [email protected] wrote:
>
> >Deal MEMS reserachers:
> >
> >        I got a problem when peel off PDMS off the
> Si mold made by DRIE since I
> >did not treat the mold before pour PDMS on. After
> that, I tried to use HF to
> >remove PDMS so that I can use the mold again. But
> it takes very long and the
> >cleaning is not complete. Can anybody give some
> suggestions how to totally
> >remove the PDMS from the Si mold? Any input is
> highly appreciated.
> >
> >
> >
> >Sincerely,
> >
> >Bo
> >
> >
> >
> >
> >_______________________________________________
> >[email protected] mailing list: to unsubscribe
> or change your list
> >options, visit
> http://www.memsnet.org/mailman/listinfo/mems-talk
> >Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> >Visit us at http://www.memsnet.org/
> >
> >
>
> --
> Alison Cleary
> Bioelectronics Group
> Electronics and Electrical Engineering
> Oakfield Avenue
> University of Glasgow
> G12 8LT
> Scotland
> UK
>
> Phone: +44 (0)141 330 2092
>
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
> http://www.memsnet.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/


__________________________________________________
Do you Yahoo!?
Yahoo! Mail Plus – Powerful. Affordable. Sign up now.
http://mailplus.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing