Brian Semak
refractive index of silicon nitride
Brian Semak
2002-11-22
Hi All

I am loking some data of the dispersion of Si3N4, that is data (a table would be
nice) on the refractive index  n of Si3N4 vs. the wave length found by
spectroscopic ellipsometry. Does anyone know where to find it, or can give me
the data

Kind regards/Med venlig hilsen

Brian S. Semak, M.Sc. Phys.
R&D Engineer
Hermetic Packaging

Hymite A/S
DTU, Bygn. 325, 1st floor
DK-2800 Lyngby
Denmark

Telephone(Direct): + 45 4525 9147
Fax:                        + 45 4525 9156
E-mail: [email protected]
www.hymite.com

***********************************************************************
This email and any files transmitted with it may contain confidential
information intended for the addressee(s) only. The information is not to be
surrendered or copied to unauthorised persons. If you have received
this communication in error, please notify us immediately by
telephone: +45 4525 9140. Thank you.
***********************************************************************




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Tanner EDA by Mentor Graphics
MEMStaff Inc.