adhesion-layers for Au evaportation onto SiN
[email protected]
2002-11-22
O2 plasma is not good for reactive metals. Cr is one of the
reactive metal. Although there is a inert Au layer on top of
it, the O2 plasma can diffuse through the Au layer into the
Cr layer and then oxidise the Cr. I have the similar
experience on Au/Ti layer.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.
The Branford Group