I have a colleague who is interested in using a LPCVD nitride mask on
bare silicon wafers (one side polished) during a 10 hour KOH (45%) etch
at 85 C.  I would appreciate recommendations on the following....

a) vendor suggestions for performing the LPCVD nitride
b) minimum nitride thickness required
c) any other precations or concerns

Thanks,

--
Dr. Kevin M. Walsh
Electrical Engineering Department, Speed Scientific School
University of Louisville, Louisville, KY 40292
(502) 852-0826

Internet address: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation