1997-04-28
Mark Sheplak
Mark Sheplak
1997-04-28
The following papers may be of some help:

Tabata et al., "Anisotropic Etching of Silicon in (CH3)4OH Solutions",
Transducers '91, pg 811-814, 1991

Merlos, et al., "TMAH/IPA anisotroipic etching characterstics",
Sensors & Actuators A, Vol. 37, pg 737-743, 1993

_________________________________________________________
Mark Sheplak
Microsystems Technology Laboratories and
Department of Electrical Engineering and Computer Science
60 Vassar Street
Room 39-561
Massachusetts Institute of Technology
Cambridge, MA 02139  USA
Phone: (617)253-6761
Fax: (617)253-8806
Email: [email protected]
_________________________________________________________



------- Forwarded Message

Return-Path: [email protected]
Received: by darkstar.isi.edu (5.65c/5.61+local-25)
        id ; Mon, 28 Apr 1997 10:31:04 -0700
Received: by darkstar.isi.edu (5.65c/5.61+local-25)
        id ; Mon, 28 Apr 1997 10:31:03 -0700
Message-Id: <[email protected]>
From: [email protected]
Subject: TMAH properties
Date: Thu, 24 Apr 1997 18:04:58 -0700 (PDT)
To: [email protected]
X-Url: http://mems.isi.edu/mems.html
Reply-To: [email protected]

Hi everyone,

Does anyone know about the effect of TMAH selectivity of Silicon to
Silicon oxide with change in the TMAH concentration ?

I have not been able to find any paper which documents this, although
there a quite a few papers which talk about TMAH undercutting,
improving surface quality, decreasing Al etch etc..

Any pointers will be greatly appreciated....

Thanks...

Manish Mehta
email: [email protected]




------- End of Forwarded Message


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics