Edward,
I can supply the 100um wafers but think that processing the 100um
through the Silicon Nitride process might be difficult due the low
thickness of the wafers. I can check with a few of the film houses to
see if they can provide this service on such thin wafers.
One of them is process Specialities.

Contact me off-line via email or phone.

Regards,
Ken Smith

Edward Castellana wrote:
> Hello,
>
> Does anyone know of a company that supplies double side polished wafers,
> ~100 um thick silicon, <100> wafers with silicon nitride on one or both
> sides.  I have had no luck finding one.
>
> Thanks,
>
> Ed Castellana
> Department of Chemistry
> Texas A&M University
> College Station TX  77843
>
> 979-845-7638
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


--


Kmbh Associates
47 Rocket Circle
Rancho Cordova, CA 95742  U  S  A
510-714-5055 Efax- 510 217 4421 or 561 658 6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications. Service in SOI, Polishing SSP and DSP.
Quartz, Glass, Pyrex and Borofloat Wafer Supply. Anodic Bonding. SOG, SOS.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMStaff Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing