Kevin M. Walsh
1um LPCVD nitride
Kevin M. Walsh
1997-05-05
I am looking to have about 50 wafers (4 inch) coated with 1.1um +/- .1 um
of LPCVD SiN.  From the literature, this seems possible if a silicon rich
SiN is used to reduce internal stress.  If anyone knows of a vendor that
can do this, I would appreciate the information.

Thanks,

--
Dr. Kevin M. Walsh
Electrical Engineering Department, Speed Scientific School
University of Louisville, Louisville, KY 40292
(502) 852-0826

Internet address: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Mentor Graphics Corporation
MEMS Technology Review