MEMSnet Home: MEMS-Talk: thick photoresist for dry etching
thick photoresist for dry etching
2002-12-16
[email protected]
2002-12-16
Mihaela Balseanu
2002-12-17
[email protected]
thick photoresist for dry etching
[email protected]
2002-12-17
I would recommend SU-8 resist by MicroChem. I have been using it for deep
silicon etch and it has higher selectivity properties than any of the positive
resists. They make a special formulation for us that is about 5 microns thick.
At this thickness we have been able to produce anisotropic profiles easily which
translates into steep sidewalls in single crystal silicon. Call Mark Shaw at
617-965-5511 x 308 and tell him Bob Henderson recommended him. Bob

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
The Branford Group