Greg Miller
2002-12-18
Hi Lakshmi,

Try Silicon rersource (480-503-4564) - they have an adhesion promoter siimilar
to HMDS but specially tailor to gold. It should do the trick.

Thanks,

Greg Miller
KVH Industries
Email: [email protected]



-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of lakshmikanth namburi
Sent: Tuesday, December 17, 2002 5:31 AM
To: [email protected]
Subject: [mems-talk] hydrophobic gold


I am looking for a chemical that would make gold hydrophobic. For
example when gold is in contact with strong acids it turns hydrophilic.
Is there a way to reverse this? Any help is greatly appreciated.
-Lakshmi Namburi.

__________________________________________________
Do you Yahoo!?
Yahoo! Mail Plus - Powerful. Affordable. Sign up now.
http://mailplus.yahoo.com

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.
University Wafer