MEMSnet Home: MEMS-Talk: Ohmic contacts
Ohmic contacts
2002-12-19
Milan Buncick
2002-12-20
[email protected]
Ohmic contacts
Milan Buncick
2002-12-19
Folks,
        Can someone provide me with a recipe for making ohmic contacts on n type
Si
with Au as the top layer.  I know that this should be a rather straight
forward and well documented procedure but we have had lots of trouble
getting good contacts.
Thanks,
Milan

Dr. Milan Buncick
Director, MEMS/Photonics
The AEgis Technologies Group Inc.
631 Discovery Drive
Huntsville, AL 35806
(256) 876-7457
(256) 842-2507 Fax
"To have a friend you must be a friend" - Snoopy


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Tanner EDA by Mentor Graphics
The Branford Group