Dear Mems-Talk Users,

We experienced some shrinkage problems with the S1828 (spun and softbaked)
photoresist after dipping it into Bromine Methanol (1:100).  Can anybody suggest
an alternative photoresist for such harsh etchants as Br:MeOH ?

Thanks from now and happy new years,

Oray Orkun Cellek
[email protected]
Research Assistant, Ph. D. Student
Electrical & Electronics Engineering Department
Middle East Technical University
06531 Ankara
Turkey
Tel : +90 312 210 4579
Fax : +90 312 210 1261



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
The Branford Group
Mentor Graphics Corporation