Mr. Lee,
  One method to produce thin, uniform layers is by using an energetic
ion beam for deposition. It is possible to modify standard sputtering
systems to produce a negative ion beam. Conversion kits are available
from www.plasmion.com .

-Mike

>>> [email protected] 12/30/02 07:38 AM >>>
Sputtered W and Mo  can meet constant 100~200A film thickness in whole
substrate area ?



i'm worry about bad coverage on substrate due to very thin thickness.



If impossible , how about using electoplating process?



Happy New Year...

TW Lee.



==================================================

/ aero MEMS Laboratory ,

/ School of Mechanical & Aerospace Engineering,

/ Seoul National University , KOREA

/

/ C.P : 016 - 459 - 3024

/ Lab : 02 - 880 - 1728



_______________________________________________

[email protected] mailing list: to unsubscribe or change your list

options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.

Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
University Wafer