MEMSnet Home: MEMS-Talk: au-si bond
au-si bond
2002-12-23
bei
2003-01-06
Luesebrink Helge (2 parts)
au-si bond
Luesebrink Helge
2003-01-06
Liubei,

MIT is successfully bonding Au-Si with an EVG501 wafer bonding system - check
out http://www.electrochem.org/meetings/past/200/abstracts/symposia/p1/1471.pdf

Looking forward to hearing from you soon.
With very best regards,

Helge W. Luesebrink

EV Group, Inc. - Regional Sales Manager -Tel: (401) 784 0008; Fax: (401) 784
9933; e-mail: [email protected] ; Web site: www.EVGroup.com



-----Original Message-----
From: bei [mailto:[email protected]]
Sent: Friday, December 20, 2002 1:41 AM
To: [email protected]
Subject: [mems-talk] au-si bond


Hi,

Does anyone have experiences with Au-Si bonding?I have done  expriments for
several times under different temperatures(from 350oC  to  420oC),but bad
results:(.What are there others reasons that influence on bonding quality except
temperature,totle thickness variation? The most I am wondering is the wafer
surface,but I still have no idea to pretty solve it,and I wish it has >80%
bonding possibility.
And any advice will be appreciated.

Best Regards

liubei

[email protected]


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
Luesebrink Helge.vcf (text/x-vcard, 443 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing