MEMSnet Home: MEMS-Talk: Re: Looking for glass paste suppliers
Re: Looking for glass paste suppliers
2003-01-08
Gabriel, Markus
Re: Looking for glass paste suppliers
Gabriel, Markus
2003-01-08
Jalinous,

I know two of them: Ferro and Schott, both deliver ready mixed pastes. I
heard about an other supplier in Japan, but don“t know the name. For further
information you can contact me.

SUSS supplies SUbstrate bonders, just in case you need the paste for wafer
bonding. We offer also demos and other services.

Regards,
Markus.


SUSS MicroTec
Business Field MEMS
Markus Gabriel
Schleissheimer Str. 90
85748 Garching
Germany
Fon     +49 89 32007 - 313
Fax     +49 89 32007 - 390
email   [email protected]
http://www.suss.com/mems



Date: Mon,  6 Jan 2003 17:12:51 -0500
From: "Jalinous Esfandyari" 
To: 
Subject: [mems-talk] Looking for glass paste suppliers
Message-ID: <[email protected]>
Content-Type: text/plain; charset=us-ascii
MIME-Version: 1.0
Precedence: list
Reply-To: [email protected], General MEMS discussion
        
Message: 5

Hi Everyone,

I am looking for companies who produce and/or provide glass paste with low
melting temperature (400 to 650C). The geographical location of the company
is not an issue.


Your help would truly be appreciated.


Regards,

Jalinous Esfandyari, Ph.D.
Intelligent MEMS Design, Inc.
Tel: (613) 596-9686
Email: [email protected]
2830 Haughton Ave.
Ottawa, ON, K2B 6Z3
www.imemsdesign.com
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Nano-Master, Inc.
Tanner EDA by Mentor Graphics