Jack,

  It sounds to me like the area that you need to concentrate on is cleaning.
The PDMS should bond well directly to very clean Si or glass.  Particulates will
cause voids in your bond.  Another thing to look into is plasma oxidation just
prior to attempting the wafer bond, in order to get a better oxide layer for the
bond.

Regards,

Brian Douglas
Suss Microtec Inc.
Applications Engineer - Bonders
Phone: (802) 244 - 5181 x202
Fax:  (802) 560 - 0001

BRIAN DOUGLAS.vcf (text/x-vcard, 606 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review
University Wafer