Dicing Saw Blades
David Nemeth
2003-01-08
Your final thickness, 1.5 mm, is on the order of 60 mils (0.060"), which is
just on the edge for a 2" hub style blade.  I'd use a resin blade (because
of the pyrex.)
I've found talking to the blade vendors is helpful - either disco or K&S
(http://www.kns.com/prodserv/Dicing/blade-form.asp).
To browse info about blades, try:
http://www.kns.com/prodserv/literature/dicing.asp

Good luck,

David Nemeth
Senior Process Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Cormac Eason
Sent: Tuesday, January 07, 2003 1:30 PM
To: [email protected]
Subject: [mems-talk] Dicing Saw Blades


Hi all,

Could anyone recommend a dicing saw blade or blades suitable for cutting
the following combinations of materials:

Silicon (0.5mm thick) anodically bonded to Pyrex (0.5mm thick)

Pyrex (0.5mm thick) spin coated with a 5 micron layer of SU 8

Silicon (0.5mm), with an electroplated Copper layer (0.4mm), topped with a
5 micron thick SU 8 layer and a 0.5mm Pyrex layer.

Thicknesses are approximate at the moment, but the maximum depth to which
I'll be cutting will be < 1.5mm

The thickness of the blade doesn't matter to me as there is plenty of room
between samples, though the more vertical the cut edges are the better.
Thanks in advance for all assistance.
--

Regards,
Cormac Eason


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
University Wafer
Addison Engineering