MEMSnet Home: MEMS-Talk: removeing a negative pr on Si(100) wafer
removeing a negative pr on Si(100) wafer
2003-01-08
Kim, Gunwoo
2003-01-09
Mighty Platypus
removeing a negative pr on Si(100) wafer
Mighty Platypus
2003-01-09
Hello Gunwoo,
Piranha foolwed by BOE will give you a "perfect" Si wafer. Of course,
your dots may be gone as well. What are these dots made of? What is on
your wafer that you *don't* want to strip?


Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Never worry again about the quality of your random numbers!"
    -- Advertisement

On Wed, 8 Jan 2003, Kim, Gunwoo wrote:

>  Dear all.
>
> I have a little problem.
> I am using a negative pr to make a dot pattern.
> However, after removing pr process using RR4(Dimethyl Sulfoxide) and acetone,
I can still see remained pr within 100nm size on a wafer and around dot
patterns. I tried to remove the pr using extra NMP cleaning step, but still I
can see the pr.
> Would you recommend how can I remove all of the pr within 100nm size and how
can I make a perfect si wafer after cleaning step? It is very important for me
because this process wafer will be moved to MBE chamber without any defect
including remained pr or particles around dot patterns.
> Thank you for your attention.
>
> Best regards,
> Gunwoo Kim
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
MEMS Technology Review
Mentor Graphics Corporation