Anyone know a good nickel etch?
Carl Arft
2003-01-09
I'm trying to pattern nickel with photoresist.  Aqua regia seems to etch
too quickly, and leaves some nickel un-etched.  Anyone have any other etch
chemistries?

thanks

please respond to:  [email protected]



********************************************
Carl Arft
Dept. of Electrical and Computer Engineering
University of California, Davis
Email: [email protected]
Phone: (530) 754-9249
********************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
The Branford Group
Nano-Master, Inc.