A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Dry strukturing of tungsten with PR as mask
Dry strukturing of tungsten with PR as mask
2003-01-15
Stefan Junge
2003-01-28
张振峰
2003-01-15
[email protected]
2003-01-15
Bill Moffat
Dry strukturing of tungsten with PR as mask
Stefan Junge
2003-01-15
Dear all,

i want to structure tungsten dry with PR as masking layer.
Does anybody have experiences on etchrates, selectivities
to SiO2. I thought about CH4, SF6 or Ar as gases.

Regards,

Stefan Junge


--
Institute for Microsensors, -actuators and -systems (IMSAS)
University of Bremen
Stefan Junge (Ph.D student)
Dep. 1: Physics/Electrical Engineering
Otto-Hahn-Allee
28359 Bremen, Germany

P.O. Box 330 440
28334 Bremen, Germany

Tel.: +49-421-218-3586
Fax.: +49-421-218-4774
E-Mail: [email protected]
Internet: www.imsas.uni-bremen.de

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review