Hi Bala,

Shipley company sells non-cyanide based gold solutions for microelectronic
and IC applications.
www.shipley.com

Regards,
David






|--------+----------------------------->
|        |          "Balaji            |
|        |          Lakshminarayanan"  |
|        |                          |
|        |          Sent by:           |
|        |          mems-talk-bounces@m|
|        |          emsnet.org         |
|        |                             |
|        |                             |
|        |          01/16/2003 01:20 PM|
|        |          Please respond to  |
|        |          General MEMS       |
|        |          discussion         |
|        |                             |
|--------+----------------------------->
  >-----------------------------------------------------------------------------
------------------------------------------|
  |
|
  |      To:     
|
  |      cc:
|
  |      Subject:     [mems-talk] Au plating solution
|
  >-----------------------------------------------------------------------------
------------------------------------------|




Hi,

I'm looking for companies (in USA) that sell Au plating solution
(non-cyanide based). Technic is one company that offers a ready-to-use
solution but I'm having problems with their solution. The surface
roughness of the plated film is difficult to control even if I have very
low current. Does anyone know other companies which have similar
products?

Thanks

Bala



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Addison Engineering
Harrick Plasma, Inc.