Re: polyimide etching
1997-06-05
Alexander Holke
Re: polyimide etching
Alexander Holke
1997-06-05
>
> I try to etch polyimide (DuPont Pyralin 2611) in a O2-plasma (RIE) and I
> always get some residue on the wafer.
> Does anybody know how to solve this problem ?
>
> Thanks in advance,
>
> Ralf
>
> ****************************************
> Dipl. Ing. (FH) Ralf Keller
>
> Fraunhofer-Institut fuer Biomedizinische Technik
> Fraunhofer Institute for Biomedical Engineering
> Ensheimer Str. 48
> 66386 St. Ingbert, Germany
> Tel.: +49 (0) 6894 / 980-158     Fax: ..-400
> e-mail: [email protected]
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMStaff Inc.
Tanner EDA by Mentor Graphics