Hi, I am doing TiO2 sol-gel spin-coating process.
The sol that I got from the precursor Ti(OC3H7)4
looks clear and I use ethanol as the solvent.
However, after spinning on the spin station usually
used in the cleanroom, I found there are very thin
streaks emanating from the center of the wafer and
they are very uniformly distributed on the entire
surface of the wafer. I changed the solvent to IPA
assuming it evaporates slower than ethanol. The
situation doesn't change.

I am wondering if it is because of the spinning
process or still due to some problems with the sol.

Thanks very much for any suggestions!

Yuan

__________________________________________________
Do you Yahoo!?
Yahoo! Mail Plus - Powerful. Affordable. Sign up now.
http://mailplus.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
MEMS Technology Review
Nano-Master, Inc.