A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Photo-definable glass
Photo-definable glass
2003-01-24
Sarah Schwab
2003-01-27
Karl Cazzini
2003-01-27
Mac McReynolds
2003-01-28
St.Clair, Loren
2003-01-28
Charles Ellis
2003-01-30
Paolo Bondavalli
2003-01-28
Bill Moffat
2003-01-30
St.Clair, Loren
Photo-definable glass
St.Clair, Loren
2003-01-30
Charles,

I have worked with glass samples I received from Schott.  I was intrigued
with two of the glasses aspects; 1) photo-patternability and 2) anodic
bondability.  I saw FOTURAN as a possible rapid prototyping material with
specific micro-fluidic applications.  The depth was easy to achieve with but
the bottoms and sidewalls were rough.  When I tried to anodic bond the
patterned glass to silicon the glass cracked rather violently, I believe due
to TCE mismatch.  TCE(FOTURAN) = 8.6 ppm and TCE(Silicon) = 2.6ppm.  I did
not use any tricks just what I leaned in the document "Fotosensitive
structuring of FOTURAN" that I received from Craig Wurzel.

Hope this helps,

Loren.

 -----Original Message-----
From:   Charles Ellis [mailto:[email protected]]
Sent:   Tuesday, January 28, 2003 2:49 PM
To:     'General MEMS discussion'
Subject:        RE: [mems-talk] Photo-definable glass

Loren,

Have you actually worked with this glass. I have found it to be almost
impossible to work with, and expensive.  If someone has a lot of
experience with this glass please let me know, I would like to learn the
"tricks".

Thanks,
Charles Ellis
Auburn University

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of St.Clair, Loren
Sent: Tuesday, January 28, 2003 7:47 AM
To: 'General MEMS discussion'; '[email protected]'
Subject: RE: [mems-talk] Photo-definable glass

Sarah,

Foturan from Schott Corporation is a material that can be patterned
using a
standard mask aligner (300-320nm) and HF.  Craig Wurzel can be contacted
at
[email protected] if you have any questions about prices.


Hope this helps,

Loren St. Clair


 -----Original Message-----
From:   Sarah Schwab [mailto:[email protected]]
Sent:   Friday, January 24, 2003 4:38 PM
To:     '[email protected]'
Subject:        [mems-talk] Photo-definable glass

Hello there
I am looking for some information on photo-definable glass.
Could anyone please help me with the following:

Suppliers?
Approx cost per wafer 4" diameter - sample quantities?
Minimum thickness?

Many thanks
Sarah


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer