film thickness
2003-02-04
[email protected]
2003-02-05
Bill Moffat
film thickness
Bill Moffat
2003-02-05
Pan,
    You need to supply more details.  Are you looking for lift off, does your
sacrificial resist have to withstand any severe process before the sacrifice.
The answers depend upon the process you wish to use.  Bill Moffat

-----Original Message-----
From: [email protected] [mailto:[email protected]]
Sent: Tuesday, February 04, 2003 2:01 PM
To: [email protected]
Subject: [mems-talk] film thickness


Dear MEMS colleague:

I would like to use photoresist as sacrifical layer with required thickness
around 0.5 um in my fabrication process. Could you tell me what kind of
photoresist I should use and where I can find their process? Thank you very
much for your help.

Best Regards,

Pan Mao



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer