Dr. Mark W. Lund
RE: General Book on Etchants
Dr. Mark W. Lund
1997-06-26
The Chemical Rubber Company (CRC) has a Handbook of Metal Etchants
which is very useful.  The "Metal" part of the title is unfortuntate
because the book includes semiconductors and many compounds.  I
have found this book to be extremely useful even (like all CRC
publications) it is very pricy.

best regards
mark

Mark W. Lund, PhD
Director             >> Soft X-ray Web page http://www.moxtek.com<<
MOXTEK, Inc.
452 West 1260 North
Orem UT 84057       801-225-0930        FAX 801-221-1121
[email protected]

"The state is good at simple tasks, like killing people and seizing their
wealth.  It has far more trouble reaching inside individuals and making them
good." Doug Bandow


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.