Dear all,

i plan to package demonstrators of an optical micro chip in a ceramic
package and seal it with an float glas with anti reflective coating (laser
application 632,8 nm). The package is DIL28 (large cavity) with 7,8 mm*7,8
mm cavity. The glas seal should be minimum 13 mm*13 mm. Does anybody know
where i can purchase 100 pieces of such glas seals in a convenient time for
a low price.

Thanks a lot for the help

Torsten Kiessling


 -------------------------------------------
Dipl.-Ing. Torsten Kießling
Fraunhofer Institute
Photonic Micro Systems
Grenzstr. 28
D-01109 Dresden

Tel.: +49(0)351/8823-283
Fax:                -266
email: [email protected]
Internet: http://www.ipms.fhg.de/
-------------------------------------------


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
MEMStaff Inc.
Process Variations in Microsystems Manufacturing