Michael D Martin
Glow plasma color & leakage in a RF Sputtering
Michael D Martin
2003-02-20
The plasma color is also influenced by the target but to determine if
you have a leak pump down to a few mTorr and valve off the pump from the
chamber. Record the pressure rise as a function of time and determine
the leak up rate. Compare this figure to the specifications of the
system. To locate the leak pum down and squirt isopropanol around the
o-rings and look for a sudden pressure rise.

-Mike

>>> [email protected] 02/17/03 08:51PM >>>
We have a BOC Edwards Auto 500 Sputtering system.  The normal glow
plasma color was light green, but it is pink. I still can deposit Au
films with lower deposition rate but not Si, instead I got transparent
films. I suspect the chamber has leakage and the Si could be oxidized.
Does anybody has the same experience? Please advice.

Bing



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.