2003-02-18
신영식
2003-02-20
Michael D Martin
About Pt etching with Aqua Regia
Michael D Martin
2003-02-20
About 85 +-2 deg. C is perfect. Though I use a slightly different
recipe: 8 H2O: 7 HCl : 1 HNO3 by volume.

Good luck,
   Mike

>>> [email protected] 02/17/03 06:21PM >>>
Dear

I'm trying to etch Pt layer on a glass wafer.
I sputtered Ti and Pt 1000A and 3000A thick respectively on a 4" glass
wafer.
I patterned with AZ1512 first and then tried to etch the Pt layer with
aqua regia( HCl:HNO3=3:1).
But I couldn't identify any etching of the Pt.

Do I need to heat the aqua regia to etch the Pt layer?
If I do not raise the temperature, can't I etch the Pt?
Then What is the proper temperature?

I hope to get your reply soon...

Thank you...
Have a nice day~~!!




Shin, Young Shik,
Master Candidate
Micro-BioMechanics Team, Advanced Machine Element Design Laboratory,
School of Mechanical & Aerospace Engineering, Seoul National
University

[email protected]   [email protected]



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review
Nano-Master, Inc.