Dear Unni,
Parylene can not be spin coated, Parylene has to applied in gaseous vacuum-
deposition.

MVH/Best regards
Kjell Askerfalk
Para Tech Coating Scandinavia AB
(Elektronikhöjden 6)
Box 567 S-175 26  Järfälla
Sweden
Tel office +46 (0)8-58082579
Tel mobile +46 (0)73-9626270

----- Original Message -----
From: 
To: 
Cc: 
Sent: Tuesday, March 04, 2003 1:46 PM
Subject: [mems-talk] Parylene dimer coating


Can anybody tell me if parylene dimer can be spin coated and =
polymerised?
Ideas about dip coating are also welcome
Unni
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review
MEMStaff Inc.